China PP Hollow grid sheet production line Manufacture Parameters:
This PP Hollow grid sheet production line Line is used to produce PP hollow/corrugated sheet. The fancy PP Hollow grid sheet production line is consisted of one or two single screw extruders, hydraulic screen changer, mould, calibration platform, six roller haul-off machine, cooling fan, corona treatment, two roller haul-off machine, cutting machine, stacker etc.
Raw Material is PP + CoCo3
Final products: PP/PC hollow corrugated sheet , PP co-extrusion corrugated sheet for cartons
Model
Sheet Thickness
Sheet Width
Extruder Type
Main Motor Power
HRS-1250
1.5-12mm
1250mm
100/36
55-75kw
HRS--1750
1.5-12mm
1750mm
120/36
75-90kw
HRS--2150
1.5-12mm
2150mm
120/36
90-110kw
HRS--2450
1.5-12mm
2450mm
120/36
90-110kw
HRS--2800
1.5-12mm
2800mm
120/36
132kw
Comrise Customized PP Hollow grid sheet production line Product Applications:
PP Hollow grid sheet produced by Comrise machinery is lightweight, impact and oil resistant, and waterproof. Applications include packaging containers, display panels, daily use items, stationery, and protective packaging for building materials. PP can be formed into any shape and type of product such as turnover boxes, component boxes and plastic partitions. This is excellent material widely used for protecting electronic parts.
What is the questions and solutions in the production process of advanced PP Hollow grid sheet production line?
Q: Why does the surface of the board appear uneven and wavy as a whole?
A: Insufficient vacuum pressure on the molding template, need to adjust the vacuum suction force.
Q: What is the reason for the wrinkle defects on the surface of the board?
A: Block of mold core air holes, need cleaning mold core air holes.
Q: Why Clustered wave patterns appear on the surface of the board?
A: Because the rapid discharge of materials from this area of the mold has caused material compression. Adjust the mold lip and fine tune the bolt.
Q: What should we do if the board is easy to flatten and lacks sufficient support?
A: The thickness of the vertical bars in the grid is insufficient. Adjust the gap between the mold lips to increase the thickness of the vertical bars.